Abstract:
In the present investigation, transient liquid-phase bonding was performed between pure titanium (Grade 2) and stainless steel (X5CrNi 18-10) using 0.1 mm thick nickel foil as an intermediate material. The process was carried out at the temperatures of: 850, 875, 900, 925, 950 and 1000 °C for 60 minutes under the compressive stress of 2 MPa in a vacuum. [..]